About The KISHO Glass Coating Hardening Time Question Mar 09, 2018

About The KISHO Glass Coating Hardening Time Question

The temperature at 25 degrees, the film surface hardening takes two days, the film is completely hardened takes about one week. During this period, try to avoid the rain and dew. In winter the temperature is relatively low, the curing time will be longer.

In addition, various heating methods can be accelerated by curing speed, the common use heat lamp, a reference time 2 hours surface layer substantially hardened.

When double superimposed Glass Coating, If you want to achieve the best results, let the first surface-hardened layer be applied. Then applying second.